Specification
|
|
|
Density | 80-90 Kgm/3 BS4443P1M2 | |||||
CompressionSet(75% 22Hrs.70oC) |
16% BS4443P1M6 | |||||
Tensile Strength | 110KPa BS4443P1M3A | |||||
Elongation at Break | 160% BS4443P1M3A | |||||
Oxygen Index | 59% BS2782P1 | |||||
BS4735 Flammibility | Does not burn, melt or drip. |
|||||
Char Formed | ||||||
EP1 Radiateur | Class M1 | |||||
Indentation Hardness Index |
308N BS4443P2M7 | |||||
Pounding Class BS3379 |
V BS4443P5 | |||||
Smoke Emission | 50% BS5111 | |||||
Temperature Working Range |
30 to 110oC Continuous | |||||
Thermal Conductivity | 0.050 Wm-1K-1 | |||||
Acoustic Specification | ASTM C384 and BS EN 20354 (previously) BS 3638 : 1963 are both Standard tests for measuring absorption coefficients. ASTM C384 is laboratory scale test measuring normal incidence coefficients. BS EN 20354 is a full scale reverberation room test, measuring random incidents coefficients. Both methods give an indication of the potential performance of the material under the test. Whilst the latter reverberation room method may prove more relevant in most practical situations, neither test can predict overall performance in a real application. | |||||
Absorption Coefficients : ASTM C384 |
||||||
Thickness (m/m ) | Frequency(Hz) | |||||
125 | 250 | 500 | 1000 | 2000 | 4000 | |
12 | 0.04 | 0.14 | 0.15 | 0.29 | 0.54 | |
25 | 0.07 | 0.14 | 0.32 | 0.80 | 0.71 | |
50 | 0.11 | 0.11 | 0.50 | 0.86 | 0.84 | 0.90 |
Absorption Coefficients : BS EN20354(BS3638) :1963 |
||||||
Thickness (m/m ) | Frequency(Hz) | |||||
125 | 250 | 500 | 1000 | 2000 | 4000 | |
12 | 0.06 | 0.09 | 0.18 | 0.29 | 0.38 | 0.58 |
25 | 0.09 | 0.22 | 0.38 | 0.52 | 0.63 | 0.73 |
50 | 0.24 | 0.47 | 0.75 | 0.84 | 0.87 | 1.02 |
100 | 0.41 | 1.01 | 1.10 | 0.96 | 1.03 | 1.06 |